Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | 2-Hydroxyethyl Methacrylate | HCID 13360 | — |
| Reactant | Stearyl acrylate | HCID 62552 | — |
| Reactant | 2,2'-Azobis(2-methylbutyronitrile) | HCID 93079 | — |
| Solvent | Ethyl Acetate | HCID 8857 | — |
| Product | Oda hema | HCID 88721785 | — |
Reaction Steps
Crosslinked compositions with low tack can be of use in particular applications. Compositions with these properties are described in the following three examples. In a glass polymerization bottle were charged 72 g IOA, 18 g octadecyl acrylate (ODA), 10 g HEMA, 150 g ethyl acetate, and 0.4 g VAZO-67 (Wako). The bottle was purged with nitrogen, sealed, and tumbled in a water bath maintained at 60° C. for 16 hrs. The resulting terpolymer, IOA/ODA/HEMA, was isolated by precipitation in petroleum ether. The terpolymer (polymer XIII) has a number average molecular weight of 26,000.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US07074858B2 |
|---|
| Source dataset | uspto-grants-2006_07 |
|---|
| ORD ID | ord-ef7d24618e704333a9b3102d27a16042 |
|---|
| Source note | uspto-grants-2006_07 |
|---|