Reaction Steps
An autoclave having an internal volume of 1 liter was charged with 228 g of xylene, and heated up to 260° C. in an atmosphere of a nitrogen gas. A mixture of 190 g of dicyclopentadiene and 190 g of styrene was added over 2 hours while being stirred. The reaction was further conducted at the same temperature for 4 hours. An unreacted monomer, a low polymer and the solvent were removed from the resulting polymer solution to obtain a dicyclopentadiene-styrene copolymer having a number-average molecular weight of 690, a softening temperature of 110° C., a bromine value of 62 g/100 g and an aromatic ring content of 46% by weight.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06538063B1 |
|---|
| Source dataset | uspto-grants-2003_03 |
|---|
| ORD ID | ord-dbb5066cb51a482dbdffb487f2304130 |
|---|
| Source note | uspto-grants-2003_03 |
|---|