Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Methacrylic Acid | HCID 4093 | — |
| Reactant | Isobutyl Methacrylate | HCID 7352 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | epsilon-CAPROLACTONE | HCID 10401 | — |
| Reactant | 2-Hydroxyethyl Methacrylate | HCID 13360 | — |
| Solvent | Ethyl Acetate | HCID 8857 | — |
| Product | Benzoyl Peroxide | HCID 7187 | — |
Reaction Steps
Subsequently, 100 parts of the resin (VIB-3) was fed into a same reaction vessel replaced with nitrogen, followed by elevating a temperature to 75° C. while agitating. There was added dropwise a mixture composed of 15.4 parts of methacrylic acid, 23.3 parts of styrene, 22.4 parts of isobutyl methacrylate, 5.5 parts of 2-hydroxyethyl methacrylate, 50.1 parts of the -caprolactone-modified acrylic monomer obtained in the Reference Example 3, 9.3 parts of “Niper BW” [benzoyl peroxide manufactured by Nihon Yushi, Ltd.], and 116.7 parts of ethyl acetate over 4 hours to allow to conduct a polymerization reaction. Also after that, agitation was allowed to continue over 4 hours to obtain a vinyl-based copolymer (VIA-5). Nonvolatile components were 48.6%.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06767987B2 |
|---|
| Source dataset | uspto-grants-2004_07 |
|---|
| ORD ID | ord-b72cea508b91433ca154f45d7033aa1d |
|---|
| Source note | uspto-grants-2004_07 |
|---|