Acrylic Acid → HCID 22481283, compound
Reaction equation
[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH3:9])(=[O:4])[CH:2]=[CH2:3].[C:10]([OH:14])(=[O:13])[CH:11]=[CH2:12].C(C1NC=CN=1)=C.[C:22]([OH:26])(=[O:25])[CH:23]=[CH2:24].[C:27]([OH:31])(=[O:30])[CH:28]=[CH2:29].[C:32]([OH:36])(=[O:35])[CH:33]=[CH2:34].[CH2:37]([C:39]([CH2:44][OH:45])([CH2:42][OH:43])[CH2:40][CH3:41])[OH:38]>>[C:1]([O:5][CH2:6][CH2:7][CH2:8][CH3:9])(=[O:4])[CH:2]=[CH2:3].[C:10]([OH:14])(=[O:13])[CH:11]=[CH2:12].[C:22]([OH:26])(=[O:25])[CH:23]=[CH2:24].[C:27]([OH:31])(=[O:30])[CH:28]=[CH2:29].[C:32]([OH:36])(=[O:35])[CH:33]=[CH2:34].[CH2:37]([C:39]([CH2:44][OH:45])([CH2:42][OH:43])[CH2:40][CH3:41])[OH:38]Participants
Procedure
A cross-linked polymeric leveling agent was prepared by mixing butyl acrylate (“BA”,40 wt %), acrylic acid (“AA”,10 wt %), vinyl imidazole (“VI”,40 wt %), trimethylolpropane triacrylate (“TMPTA”, l0 wt %) and a peroxide initiator (tert-amyl peroxypivalate) in a vessel cooled in an ice bath. The mixture was then pumped into a heated reactor containing iso-propanol alcohol as solvent. The reaction was controlled at 80° C. for approximately 2 hours. The iso-propanol alcohol was then removed by vacuum evaporation and the product was washed with water to provide an approximately 33% aqueous solution of a cross-linked polymer (BA/AA/VI/TMPTA) having an approximate weight average molecular weight (“Mw”) of 77,000, based on gel permeation chromatography against appropriate standards, and a number average molecular weight (“Mn”) of 1400.
Workup
- customA cross-linked polymeric leveling agent was prepared
- customThe mixture was then pumped into a heated reactor
- customThe iso-propanol alcohol was then removed by vacuum evaporation
- washthe product was washed with water
Sources & evidence
- ORD record
- ord-a3b55362867b42899330f0314434ca0e
- Source dataset
- uspto-grants-2013_08
- Patent number
- US08506788B2