Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Adipic Acid | HCID 196 | — |
| Reactant | Ethylene Oxide | HCID 6354 | — |
| Reactant | Diethylenetriamine | HCID 8111 | — |
| Reactant | Dimethyl Ether | HCID 8254 | — |
| Reactant | Potassium Hydroxide | HCID 14797 | — |
| Product | HCID 21983456 | HCID 21983456 | — |
Reaction Steps
The obtained polymer (179.2 g) is introduced into an autoclave and 9.29 g potassium hydroxide (50% solution in water) and 27.5 g Pluriol A 1000 E of BASF AG, Ludwigshafen (Germany), which is the monomethylether of polyethylene glycol with an average molecular weight of 1000 g/mol. The resulting mixture is flushed with nitrogen and subjected to vacuum increasing the temperature to 90° C. at 20 mbar for 2 hours to remove the water. 792 g ethylene oxide are added at 90° C. The mixture is allowed to post-react for 3 hours. The polymer composition is cooled to 80° C. and flushed with nitrogen. A brown solid is obtained (950 g), consisting of a polymer from diethylenetriamine and adipic acid with 30 mol ethylene oxide per mol NH bond.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08507613B2 |
|---|
| Source dataset | uspto-grants-2013_08 |
|---|
| ORD ID | ord-05c873d6e22e4c7d98923f1174289c22 |
|---|
| Source note | uspto-grants-2013_08 |
|---|