HRID1905351
反应详情
EQUATION
反应方程式
REACTANTS
反应物
PRODUCTS
生成物
PROCEDURE
实验过程
The white resin dispersion obtained in Production Example 2 (32 g), 2.5 g of the nigrosine dispersion obtained in Example 1, and 0.02 g of a half docosanylamide of diisobutylene/maleic anhydride copolymer were diluted with 1 liter of Isopar G to prepare a liquid developer.