HuagongsheHuagongshe Chemistry Print Report · For research reference only
Ethylene → Ethylene/Propylene 1,3-Butadiene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Ethylene | HCID 6325 | — |
| Reactant | 1,3-Butadiene | HCID 7845 | — |
| Reactant | Propylene | HCID 8252 | — |
| Product | Ethylene/Propylene 1,3-Butadiene | HCID 19841757 | — |
Reaction Steps
A polyolefin copolymer was obtained in the same manner as that of Example 1 except for changing the amount of 1,3 butadiene to 10.0 g, the polymerization temperature to 30° C., and the polymerization time to 20 minutes. The yield of the obtained polyolefin copolymer was 17.7 g. In the composition of the copolymer, the content of ethylene was 64.2% by mole, the content of propylene was 31.9% by mole, and the content of 1,3-butadiene was 3.8% by mole. The intrinsic viscosity [η] of the copolymer was 2.30 dL/g.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08188191B2 |
| Source dataset | uspto-grants-2012_05 |
| ORD ID | ord-d3b66ade2a984a6b9b262e663752e12f |
| Source note | uspto-grants-2012_05 |