Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Stearic Acid | HCID 5281 | — |
| Reactant | Magnesium monoxide | HCID 6850729 | — |
| Reactant | HCID 86758071 | HCID 86758071 | — |
| Product | Magnesium Stearate | HCID 11177 | — |
Reaction Conditions
| Temperature | 192 fahrenheit |
|---|
Reaction Steps
Product from Example 1, amounting to 50 pounds, was placed in a rotary drum dryer and was heated to 192° F. Then 0.41 pounds of commercial grade stearic acid and 0.205 pounds of magnesium oxide powder (93% passing through a 300 mesh U.S. Standard Screen) were added. The stearic acid melted, flowed onto the granules of magnesium oxychloride coated mineral supplement granules and reacted with the magnesium oxide to form a dry, solid magnesium stearate coating on the outside of the granules. The magnesium stearate coating amounted to 1.22% of the total weight of the granules.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06387412B1 |
|---|
| Source dataset | uspto-grants-2002_05 |
|---|
| ORD ID | ord-f1d69344610448b9822d9ac1a4dad808 |
|---|
| Source note | uspto-grants-2002_05 |
|---|