HuagongsheHuagongshe Chemistry Print Report · For research reference only
N,N-diethyl-m-toluamide → Urea Urethane
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | N,N-diethyl-m-toluamide | HCID 4284 | — |
| Reactant | Zytron | HCID 9299 | — |
| Reactant | Sodium Hydroxide | HCID 14798 | — |
| Reactant | Isophorone diisocyanate | HCID 169132 | — |
| Solvent | Water | HCID 962 | — |
| Solvent | Ethyl Acetate | HCID 8857 | — |
| Product | Urea Urethane | HCID 21585015 | — |
Reaction Steps
95.4 g of Rucoflex XS-5570-55, 205.8 g of Rucoflex S-1011-55 and 6.7 g of DMPA are reacted with 44.4 g of IPDI and 16.8 g of HDI at 80° C. for 3 hours to prepare a prepolymer. The prepolymer is then dispersed in a solution of 2.8 g of NaOH and 1.83 g of EA in 515.0 g of water. After 10 minutes, a solution of 1.8 g of EDA and 2.04 g of DETA is added to form an aqueous poly(urethane/urea) dispersion. A finely divided dispersion having a solids content of 39.896 and a pH of 7.2 is obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US05703158 |
| Source dataset | uspto-grants-1997_12 |
| ORD ID | ord-de1f588455034187baa26c305a3c6b1e |
| Source note | uspto-grants-1997_12 |