Methanol → HCID 86595083, compound
Reaction equation
[CH:1]([C:9]1=[CH:10][C:11]([O:13][C:14]1=[O:15])=[O:12])=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.C[OH:17]>>[CH:1](/[C:9](/[C:14]([OH:13])=[O:15])=[CH:10]/[C:11]([OH:17])=[O:12])=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1Participants
3
Conditions
- Temperature
- 100 °C
Procedure
1.8 g of the styrene-maleic anhydride polymer (molecular weight: 1600) was mixed with 5.4 g of the polyethyleneoxyglycol (molecular weight: 600). The mixture was dropped on a glass substrate and heated in an oven at 100° C. under nitrogen stream. After 30 hours, the mixture was cooled down to room temperature, immersed into methanol and dried. A thin membrane of the styrene-maleic acid polyethyleneoxy ester crosslinked copolymer of an excellent adhesive strength and mechanical strength was prepared.
Workup
- additionThe mixture was dropped on a glass substrate
- temperaturethe mixture was cooled down to room temperature
- customdried
Sources & evidence
- ORD record
- ord-68b8dcdabb4f48ecabf77603d936bffa
- Source dataset
- uspto-grants-2000_09
- Patent number
- US06123875
Reaction notes