Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Methanol | HCID 887 | — |
| Reactant | Aluminum | HCID 5359268 | — |
| Reactant | Styrenemaleic anhydride | HCID 54215275 | — |
| Product | HCID 86595083 | HCID 86595083 | — |
Reaction Steps
2.2 g of the styrene-maleic anhydride polymer (molecular weight: 1600) was mixed with 3.3 g of the polyethyleneglycol (molecular weight: 600) and 7.8 g of polyethyleneglycol monomethyl ether (molecular weight: 750). The mixture was dropped on an aluminum plate and heated in an oven at 100° C. under nitrogen stream. After 30 hours, the mixture was cooled down to room temperature, immersed into methanol and dried. An ion-conducting thin membrane of styrene-maleic acid polyethyleneoxy ester crosslinked copolymer of an excellent adhesive strength and mechanical strength was prepared.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06123875 |
|---|
| Source dataset | uspto-grants-2000_09 |
|---|
| ORD ID | ord-c0f2b6c8ab954992afaa8eb83cea0446 |
|---|
| Source note | uspto-grants-2000_09 |
|---|