A butylacrylate/styrene latex is prepared by emulsifying by stirring in the presence of the wetting agent a mixture of 18.6 g of butylacrylate and 21.2 g of styrene in 50 g of water and initiating the polymerisation, at 70° C. under nitrogen, with 0.13 g of sodium persulphate. The latex so prepared contains 47% by weight of solids.