Methanol → HCID 131714193, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methanol | HCID 887 | — |
| Reactant | Epoxide resin | HCID 16213861 | — |
| Product | HCID 131714193 | HCID 131714193 | — |
Reaction Steps
150 g ammonium polyphosphate (EXOLIT 263) was suspended in 600 ml methanol in a stirring apparatus made of glass, and the suspension was heated to gentle boiling. Next, a methanolic epoxide resin/epoxide resin hardener-solution which was prepared by dissolving 3 g BECKOPOX EP 128 and 3 g BECKOPOX VEH 2130 in 100 ml methanol was added dropwise within 15 minutes. For hardening the epoxide resin, the suspension was stirred for 2 hours while the methanol boiled gently. After cooling, the whole was filtered and the resulting filter cake was dried at 110° C. in a stream of nitrogen. 154 g treated ammonium polyphosphate which contained 3.5 mass % epoxide resin was obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04514328 |
| Source dataset | uspto-grants-1985_04 |
| ORD ID | ord-a06016a340254cc3935b3527fd0c0193 |
| Source note | uspto-grants-1985_04 |