Into 1.8 liters of ethyl cellosolve, 90 g of polymer obtained by the addition reaction of pentaerythritol triacrylate to the partial alcoholysis product of copolymer of styrene/maleic acid anhydride (styright CM-2L manufactured by Sankyo Chemical Co., Ltd.), 10 g of partial hydrolysed product of polymethyl methacrylate and 100 g of trimethylolpropane triacrylate were dissolved followed by adding the initiator of 2 g of compound a-1, 16 g of compound b-1 and 6 g of compound c-1 and 1.5 g of the coloring agent of Victoria pure blue to prepare the photosensitive solution. The photosensitive plate was produced from the solution thus prepared in accordance with the same procedures as in Example 1.