Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 1990691Generated: October 29, 2026

Toluene → 1-(2-Methylpropyl)-1,1,3,3-tetramethyldisiloxane

https://huagongshe.com/reaction/1990691

Reaction equation

Participants

RoleNameHCIDCharge
ReactantTolueneHCID 1140—
ReactantIsobutyleneHCID 8255—
ReactantTetramethyl disiloxaneHCID 57376941—
CatalystChlorotris(triphenylphosphine)rhodium(I)HCID 84599—
Product1-(2-Methylpropyl)-1,1,3,3-tetramethyldisiloxaneHCID 123394717—

Reaction Conditions

Temperature65 °C

Reaction Steps

An 80 mL Fischer-Porter high pressure bottle was charged with tetramethyldisiloxane (10.0 g), toluene (10.0 g) and Wilkinson's catalyst ((PPh3)3RhCl, 40 ppm), stirred and brought to 60° C. The bottle was attached to a manifold and pressurized with isobutylene (25 psig) and maintained at 60-70° C. for 8h. The pressure was vented, and the reaction was sampled for GC analysis; found residual tetramethyldisiloxane, M′MR product and MRMR byproduct (2:95:3). The resulting material was stripped under vacuum (approx. 150 mm Hg) at 40° C. to remove olefin and M′M′, then filtered with Celite to yield 21.3 g M′MR product/toluene solution, 94% GC purity. This product was found to have an Si—H content of 11 cc H2/g by gasiometric titration.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07645720B2
Source datasetuspto-grants-2010_01
ORD IDord-2830bb4891884cc7836192470d4b5ab3
Source noteuspto-grants-2010_01