A suspension of 20 parts of phenol and 0.6 part of ion exchange resin is prepared in a stirred reactor at 85° C. and 1 bar pressure, whilst stirring at 500 rpm, and 7 parts of isobutylene are passed in. The ion exchange resin is a sulfonated styrene/divinylbenzene copolymer resin, which has been dehydrated under reduced pressure for 20 hours at 100° C. before being used; it has a gel structure and its particle size is from 20 to 150 micrometers. The suspension is then stirred constantly in the reactor at 500 rpm. After 6 hours, 2.5 parts of phenol and 380 parts by volume of isobutylene are introduced per hour at 115° C. and 1 bar pressure and correspondingly 3.5 parts per hour of suspension are filtered through a suction line equipped with a metal filter (pore diameter 10 micrometers) and subjected to fractional distillation. After 200 hours' operation, 316 parts (88% of theory, based on starting material II) of 4-tert.-butylphenol of boiling point 143°-145° C./50 millibars are obtained, accompanied by 19.8 parts (5.5% of theory, based on starting material II) of 2-tert.-butylphenol and 9.9 parts (6.5% of theory, based on starting material II) of 2,4-di-tert.-butylphenol. The conversion is 60% of theory, based on phenol employed. The starting material II is consumed practically quantitatively.

WORKUP

后处理

  1. customis prepared in a stirred reactor at 85° C.
  2. waitAfter 6 hours
  3. filtration1 bar pressure and correspondingly 3.5 parts per hour of suspension are filtered through a suction line
  4. customequipped with a metal
  5. filtrationfilter (pore diameter 10 micrometers)
  6. distillationsubjected to fractional distillation