Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2055064Generated: October 30, 2026

Sulfuric Acid → HCID 19083679, compound

https://huagongshe.com/reaction/2055064

Reaction equation

Participants

RoleNameHCIDCharge
ReactantSulfuric AcidHCID 1118—
ReactantAzobisisobutyronitrileHCID 6547—
ReactantStyreneHCID 7501—
Reactant1-Methoxy-2-propanolHCID 7900—
ReactantHydroxystyreneHCID 138202—
Reactant1-(Tert-butoxy)-4-ethenylbenzeneHCID 577531—
SolventEthyl AcetateHCID 8857—
ProductHCID 19083679HCID 19083679—

Reaction Steps

A solution was prepared by dissolving 100 parts by weight, as the total amount, of p-t-butoxystyrene and styrene (molar ratio was p-t-butoxystyrene:styrene=80:20) in 150 parts by weight of propylene glycol monomethyl ether. This solution was kept under a nitrogen atmosphere at 70° C. for 10 hr with 4 parts by weight of azobisisobutyronitrile supplied to proceed polymerization. Then, sulfuric acid was added to the reaction solution, and the resultant solution was kept at 90° C. for 10 hr to covert the p-t-butoxystyrene unit into a hydroxystyrene unit through deprotection. Ethyl acetate was added to the obtained copolymer, the resultant solution was washed with water 5 times, the ethyl acetate phase was collected, and the solvent was removed to obtain p-hydroxystyrene/styrene copolymer (hereinafter, referred as “alkali soluble resin (A-1)”).

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07332254B2
Source datasetuspto-grants-2008_02
ORD IDord-b0b0b76442ad4b05b3d8cde5fcbb7f29
Source noteuspto-grants-2008_02