Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Propionic Acid | HCID 1032 | — |
| Reactant | Sodium Propionate | HCID 2723816 | — |
| Solvent | Water | HCID 962 | — |
| Product | HCID 23616613 | HCID 23616613 | — |
Reaction Steps
The procedure of example 1 was followed, 390 g of propionic acid and 500 g of sodium propionate being used and the mixture being heated to 165° C. until a homogeneous liquid mixture was obtained. The resultant comminuted solid (817 g) had a propionic acid content of 43.46% by weight and a water content of 0.19% by weight.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08293793B2 |
|---|
| Source dataset | uspto-grants-2012_10 |
|---|
| ORD ID | ord-1045e3f61494454e9033b95f1e5c8768 |
|---|
| Source note | uspto-grants-2012_10 |
|---|