Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2082108Generated: November 4, 2026

Styrene → Lytron 810

https://huagongshe.com/reaction/2082108

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
ReactantMaleic AnhydrideHCID 7923—
SolventTolueneHCID 1140—
ProductLytron 810HCID 62707—

Reaction Steps

A copolymer of 50 mol-% of maleic acid anhydride and 50 mol-% of styrene is prepared by introducing 98 parts by weight of maleic acid anhydride in 400 parts by weight of toluene into a reactor at a temperature of 60° to 70° C. After initiation with 0.7 parts by weight of azoisobutyric acid nitrile, 104 parts by weight of styrene are added within 3 hours at 60° to 70° C. The polymer obtained from the polymerisation precipitates in the reactor and may be filtered off after completed polymerisation and washed. The polymer contains 48.5% by weight of maleic acid anhydride units and has a Staudinger Index in acetone of [μ]=0.22 dl/g.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS05187231
Source datasetuspto-grants-1993_02
ORD IDord-c7bb44704f424cd2bf9ac220332f50c7
Source noteuspto-grants-1993_02