HuagongsheHuagongshe Chemistry Print Report · For research reference only
Methyl Methacrylate → Benzene, ethenyl-, polymer with 1,3-butadiene
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methyl Methacrylate | HCID 6658 | — |
| Reactant | 1-Bromonaphthalene | HCID 7001 | — |
| Product | Benzene, ethenyl-, polymer with 1,3-butadiene | HCID 62697 | — |
Reaction Steps
In the above example, the matrix phase must have about the same R.I. as the grafted rubber phase. The 80 percent by weight of matrix phase must be a blend of SAN and PMMA that matches the graft rubber phase having an R.I. of about 1.5390. A blend of about 42 percent of PMMA and 58 percent of SAN (76/24) was found to have a R.I. about 1.5385 matching the graft copolymer closely, giving a low haze polyblend. The refractive index was determined by an Abbe Refractometer with bromonapthalene as the immersion fluid using ASTM D-2225 at 25° C. The haze values were determined by: ##EQU1##
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04083896 |
| Source dataset | uspto-grants-1978_04 |
| ORD ID | ord-8bc5e2cce3dc48c7bd0782f685c76985 |
| Source note | uspto-grants-1978_04 |