HRID2108143

反应详情

EQUATION

反应方程式

HRID 2108143 的结构方程式

PROCEDURE

实验过程

Example 1 was repeated except that a mixture of methacrylic acid, ethylbenzene and 100 ppm, based on methacrylic acid, of p-methoxyphenol was used instead of the methacrylic acid/ethylbenzene mixture fed to the second and third polymerization vessels. Styrene/methacrylic acid copolymer was obtained at a rate of 3.2 kg per hour.

WORKUP

后处理

  1. customthird polymerization vessels