Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Citric Acid | HCID 311 | — |
| Reactant | Oleic Acid | HCID 445639 | — |
| Reactant | Zinc Oxide | HCID 3007857 | — |
| Solvent | Water | HCID 962 | — |
| Product | ZINC OLEATE | HCID 6436086 | — |
Reaction Steps
A quantity of 35 grams of Pamolyn 100, a high purity oleic acid containing about 90% oleic acid, was added gradually to a stirred slurry of zinc oxide (5.4 grams), citric acid (0.05 gram), Witconate 90 (1.18 grams), and water (60 grams) at 65° C. The mixture was stirred at 55-65° C. for 10 minutes to give a quantitative yield of zinc oleate as indicated by the infrared spectrum of the dried product.