Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2121282Generated: November 1, 2026

Stearic Acid → Zinc Stearate

https://huagongshe.com/reaction/2121282

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStearic AcidHCID 5281—
ReactantZinc OxideHCID 3007857—
ProductZinc StearateHCID 11178—

Reaction Conditions

Temperature60 °C

Reaction Steps

A slight stoichiometric excess of stearic acid was added to the zinc oxide aqueous slurry. It was heated with agitation to 60° C. to melt the stearic acid. As the melt temperature is approached, the stearic acid reacted with the zinc oxide to produce fine particle size zinc stearate. Fine particle size zinc stearate is used in the rubber and paint industries.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06696029B1
Source datasetuspto-grants-2004_02
ORD IDord-7a66b4db323142b49aeb0477acb0e38d
Source noteuspto-grants-2004_02