Sodium Silicate → Sodium orthosilicate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Sodium Silicate | HCID 23266 | — |
| Reactant | Sodium Phosphate, Dibasic, Dihydrate | HCID 6451167 | — |
| Product | Sodium orthosilicate | HCID 26051 | — |
Reaction Steps
1104 g of disodium hydrogenphosphate dihydrate are dissolved in 50 kg of water glass having the composition as in Example 1, and the solution is spray-dried in a laboratory spray dryer (spray tower) from Anhydro to give an amorphous sodium silicate having an active substance content of about 83%. 15 kg of the amorphous sodium silicate are heat-treated at 720° C. for 90 min in a muffle furnace (Nabertherm, model W1000/H). The chilled product (about 10 kg) is pulverized using a jaw crusher and a disk mill.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US06407055B1 |
| Source dataset | uspto-grants-2002_06 |
| ORD ID | ord-aa4f334fae8d48c6b15e19c293ea3ad8 |
| Source note | uspto-grants-2002_06 |