Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Carbon Dioxide | HCID 280 | — |
| Reactant | Phosphoric Acid | HCID 1004 | — |
| Reactant | Potassium Hydroxide | HCID 14797 | — |
| Reactant | Zirconium, (mu-(carbonato(2-)-kappaO:kappaO'))dihydroxydioxodi- | HCID 22645944 | — |
| Catalyst | Hafnium | HCID 23986 | — |
| Solvent | Water | HCID 962 | — |
| Product | Zirconium phosphate | HCID 160986 | — |
Reaction Steps
0.67 moles of zirconium basic carbonate (3ZrO2.CO2.xH2O) containing 2.1% hafnium composed of particles wherein a median particle size thereof was 18 μm and particles with a particle size of 0.8 μm to 50 μm were present at 100% on a volume basis of the total particles were suspended in 300 ml of deionized water, and 0.27 moles of phosphoric acid were added thereto with stirring. A 20% aqueous solution containing 0.07 moles of potassium hydroxide was further added thereto, followed by heating and aging for 2 hours at 98° C. Then, the resulting solid was sufficiently washed with deionized water in a ceramic filter washing machine until an electric conductivity of the filtrate reached 300 μS or less and the solid was taken out and dried at 120° C. for 3 hours.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08333833B2 |
|---|
| Source dataset | uspto-grants-2012_12 |
|---|
| ORD ID | ord-a366c5bf1e81464bb1fa84ae3a216d56 |
|---|
| Source note | uspto-grants-2012_12 |
|---|