HuagongsheHuagongshe Chemistry Print Report · For research reference only
Styrene → Styrenemaleic anhydride
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Maleic Anhydride | HCID 7923 | — |
| Reactant | Ammonium Hydroxide | HCID 14923 | — |
| Solvent | Water | HCID 962 | — |
| Product | Styrenemaleic anhydride | HCID 54215275 | — |
Reaction Steps
Polymers of hydrolyzed styrene-maleic anhydride and starch were prepared according to the following process: Three or six parts of starch and one part SMA 3000 (styrene-maleic anhydride copolymer sold by Arco Chemical Company, having a ratio of styrene or maleic anhydride of 3:1, a molecular weight of 1900 and an acid number of 275) were added to and heated in water for 45 minutes at a temperature of 160° F. with stirring. Then 0.88 parts of 28% ammonium hydroxide (per part of SMA) was added with mixing for an additional 20 minutes and the final pH was adjusted to 9.5 with additional ammonium hydroxide resulting in binders having about a 25% solids content. Four polymers prepared by this process are shown in Table I.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04361669 |
| Source dataset | uspto-grants-1982_11 |
| ORD ID | ord-1c276b7ceee14decbba62289a33874f2 |
| Source note | uspto-grants-1982_11 |