HuagongsheHuagongshe Chemistry Print Report · For research reference only
Methane → HCID 178419113, compound
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methane | HCID 297 | — |
| Reactant | Silicon carbide | HCID 9863 | — |
| Reactant | Boron carbide | HCID 123279 | — |
| Reactant | Titanium oxide (Ti3O) | HCID 162651 | — |
| Solvent | Methanol | HCID 887 | — |
| Product | HCID 178419113 | HCID 178419113 | — |
Reaction Steps
To the boron carbide powder, 14.5 mol % of the submicron-size or nano-size titanium dioxide powder and 21.5 mol % of carbon black were incorporated, and using a methanol solvent, mixing was carried out by a planetary ball mill made of silicon carbide (SiC) at a rotational speed of 270 rpm for 1 hour, followed by drying by a evaporator and further by drying at 150° C. for 24 hours. Then, the mixture was sieved through a sieve with an opening of 250 μm to obtain a boron carbide-titanium dioxide-carbon mixed powder.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US07417002B2 |
| Source dataset | uspto-grants-2008_08 |
| ORD ID | ord-527f550cf19a465ea96d73a4b1382069 |
| Source note | uspto-grants-2008_08 |