Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2220040Generated: October 30, 2026

Styrene → HCID 86600775, compound

https://huagongshe.com/reaction/2220040

Reaction equation

Participants

RoleNameHCIDCharge
ReactantStyreneHCID 7501—
ReactantLauryl MethacrylateHCID 8906—
ReactantDocosyl acrylateHCID 87565—
SolventTolueneHCID 1140—
ProductHCID 86600775HCID 86600775—

Reaction Conditions

Temperature60 °C

Reaction Steps

Toluene (15 g), behenyl acrylate (15 g), lauryl methacrylate (2 g), and styrene (2 g) are charged to a reactor equipped with a stirrer, a heater, a thermometer, and a nitrogen-bubbling duct. The reactor is flushed with nitrogen gas and sealed. The reactor is heated to 60° C. and 2,2′-azobis(2-methyl, ethyl-propionitrile) (0.06 g) is added. The reaction mixture is heated in the closed system at 85° C. for three hours to provide behenyl acrylate/lauryl methacrylate/styrene polymer having a number average molecular weight 34,600 Daltons with polydispersity 2.1. The viscosity of the polymer is 40 cP at 20° C. as a 40% solution in toluene.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07417009B2
Source datasetuspto-grants-2008_08
ORD IDord-3aed2ef898144713b5fe6b5dbe7f0131
Source noteuspto-grants-2008_08