Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2220043Generated: October 31, 2026

Lauryl Methacrylate → HCID 86600778, compound

https://huagongshe.com/reaction/2220043

Reaction equation

Participants

RoleNameHCIDCharge
ReactantLauryl MethacrylateHCID 8906—
ReactantDocosyl acrylateHCID 87565—
SolventO-XyleneHCID 7237—
ProductHCID 86600778HCID 86600778—

Reaction Conditions

Temperature60 °C

Reaction Steps

Xylene (15 g), behenyl acrylate (15 g) and lauryl methacrylate (2 g), are charged to a reactor equipped with a stirrer, a heater, a thermometer and a nitrogen-bubbling duct. The reactor is flushed with nitrogen gas and sealed. Then vinyl acetate (2 g) is charged. The reactor is heated to 60° C. and 2,2′-azobis(2-methyl, ethyl-propionitrile) (0.06 g) is added. The reaction mixture is heated in the closed system at 80° C. for two hours to provide behenyl acrylate/lauryl methacrylate/vinyl acetate polymer having a number average molecular weight of 47,750 Daltons with polydispersity 4.5. The viscosity of the polymer is 168 cP at 20° C. as a 40% solution in toluene.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07417009B2
Source datasetuspto-grants-2008_08
ORD IDord-df306f933b594fc1aa54f40d4798c487
Source noteuspto-grants-2008_08