Tetrahydrofuran → p-methylcarbonylstyrene

https://huagongshe.com/reaction/2227684

Reaction equation

Participants

RoleNameHCIDCharge
ReactantTetrahydrofuranHCID 8028—
Reactant1-(Tert-butoxy)-4-ethenylbenzeneHCID 577531—
ReactantCID 53628100HCID 178418400—
Productp-methylcarbonylstyreneHCID 10909702—

Reaction Steps

A 1-liter flask was charged with 500 ml of tetrahydrofuran as a solvent and 0.01 mol of sec-butyl lithium as an initiator. To the solution at −78° C. was added 30 g of p-tert-butoxystyrene. With stirring, polymerization reaction was effected for 30 minutes. The reaction solution turned red. For producing a branched polymer, 0.005 mol of p-methylcarbonylstyrene was added to the reaction solution whereupon reaction was effected for 5 minutes. Further 15 g of p-tert-butoxystyrene was added. With stirring, polymerization reaction was effected for 30 minutes. Polymerization was stopped by adding 0.1 mol of methanol to the reaction solution.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS06414101B1
Source datasetuspto-grants-2002_07
ORD IDord-c395390d019f4a399257ec06c13a5fea
Source noteuspto-grants-2002_07