Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Hydrochloric Acid | HCID 313 | — |
| Reactant | Toluene | HCID 1140 | — |
| Reactant | Methyl Methacrylate | HCID 6658 | — |
| Reactant | Oxirane, 2-[(octadecyloxy)methyl]- | HCID 61831 | — |
| Solvent | Acetone | HCID 180 | — |
| Product | HCID 86586156 | HCID 86586156 | 61% |
Reaction Steps
50 mL of Catalyst B and 32.6 g of stearyl glycidyl ether (SGE) were added to 210 mL of toluene, and a vessel was closed with the stopper. Then, the polymerization was carried out at 100° C. for 6 hours. The vessel was left to be cool to 40 ° C., and then opened. 25.0 g of methyl methacrylate was added, and the vessel was closed with the stopper. The polymerization was further carried out at 120° C. for 6 hours. The reaction solution was added to a large amount of acetone containing a small amount of a dilute solution of hydrogen chloride. A precipitated solid was dried under reduced pressure at 80° C. for 24 hours to obtain a poly(stearyl glycidyl ether/methyl methacrylate) copolymer. Colorless solid. Yield 61%.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US06417323B1 |
|---|
| Source dataset | uspto-grants-2002_07 |
|---|
| ORD ID | ord-c013f1735f16408a8e584bed69b1ea0b |
|---|
| Source note | uspto-grants-2002_07 |
|---|