HuagongsheHuagongshe Chemistry Print Report · For research reference only
Methyl vinyl ether → Methyl vinyl ether
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methyl vinyl ether | HCID 7861 | — |
| Reactant | Maleic Anhydride | HCID 7923 | — |
| Solvent | Water | HCID 962 | — |
| Product | Methyl vinyl ether | HCID 7861 | — |
| Product | Maleic Acid | HCID 444266 | — |
Reaction Steps
Copoly(methyl vinyl ether:maleic anhydride)(50:50) (Grantrez AN-119 available from GAF)(20.6 grams) was suspended in 80 grams of water and heated on a steam bath to form a 20% solids clear solution of copoly(methyl vinyl ether:maleic acid) (50:50) in water. To 61.8 grams of the solution (containing 12.4 grams of copolymer and 8.26 grams (0.072 mole) of maleic acid)) was added 4.0 grams (0.072 mole) of potassium hydroxide in order to half-neutralize all maleic acid present. Glycerol (9.3 grams) was also added as a plasticizer. The impedance of a bioelectrode prepared with the material was 33 Kohms.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04352359 |
| Source dataset | uspto-grants-1982_10 |
| ORD ID | ord-3aae0e6382004311ad259d73daea250a |
| Source note | uspto-grants-1982_10 |