HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2234274Generated: October 31, 2026
Potassium Hydroxide → HCID 131728108, compound
https://huagongshe.com/reaction/2234274
Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Potassium Hydroxide | HCID 14797 | — |
| Reactant | Bentonite | HCID 71586775 | — |
| Product | HCID 131728108 | HCID 131728108 | — |
Reaction Steps
First, the alkali-treated solid support was prepared in the following manner. 3 grams of a support (alumina, montmorillonite K-10, kaolin) was added to 4 ml of a 25% KOH aqueous solution. This mixture was irradiated with ultrasound (42 kHz) for 4 hours. Next, with an aspirator (produced by TOKYO RIKAKIKI), moisture was removed from this mixture by filtration in a reduced pressure environment. With a 500 W home-use microwave oven (EM-LAI produced by SANYO), the solid support thus obtained was irradiated with microwave of 2.45 GHz for 15 minutes. After this microwave irradiation treatment, the alkali-treated solid support was pounded finely with a mortar. In this way, three kinds of alkali-treated solid supports (alumina/KOH, montmorillonite K-10/KOH, and kaolin/KOH) were obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US07709678B2 |
|---|
| Source dataset | uspto-grants-2010_05 |
|---|
| ORD ID | ord-8a3fe988e8974458a9ae0dbe44f169e9 |
|---|
| Source note | uspto-grants-2010_05 |
|---|