Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Vinylidene chloride | HCID 6366 | — |
| Reactant | Ethene;ethenyl acetate | HCID 175988 | — |
| Reactant | Pyrophosphate | HCID 644102 | — |
| Product | Vinylidene chloride | HCID 6366 | — |
| Product | Methyl Acrylate | HCID 7294 | — |
Reaction Steps
Examples 1-8 are repeated with the following exceptions. Instead of using the PVdC set forth in Table I, a pellet having the following composition is employed: the pellet contains about 96.5 weight percent of a vinylidene chloride interpolymer; about 1.5 weight percent ethylene vinyl acetate; about 1.2 weight percent tetrasodiuum pyrophosphate; and about 0.8 weight percent of epoxidized soybean oil. The vinylidene chloride interpolymer comprises from about 99.8 weight percent of a vinylidene chloride copolymer formed from a monomer mixture comprising 94 weight percent vinylidene chloride and about 6 weight percent methyl acrylate; and about 0.2 weight percent of epoxidized soybean oil. The vinylidene chloride copolymer has a major melting point of 165° C. and a weight average molecular weight of 90,000.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US05236649 |
|---|
| Source dataset | uspto-grants-1993_08 |
|---|
| ORD ID | ord-c9ca555d2e854f639e1bf1cb5c184f56 |
|---|
| Source note | uspto-grants-1993_08 |
|---|