Acrylamide → Prop-2-enamide;styrene
Reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9]([NH2:13])(=[O:12])[CH:10]=[CH2:11]>>[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[CH2:11]=[CH:10][C:9]([NH2:13])=[O:12]Participants
3
Reactant 2
Product 1
Procedure
Next, 40 g of styrene was added into the polymerization vessel, the mixture was stirred under the same conditions for 4 hours, and further stirring was continued with addition of 2 g of acrylamide under the same conditions for 5 hours to obtain fine particles of a styrene/acrylamide copolymer.
Workup
- stirringfurther stirring
Sources & evidence
- ORD record
- ord-e9ea466dccfc42628512a75427651477
- Source dataset
- uspto-grants-1997_08
- Patent number
- US05656506