HuagongsheHuagongshe Chemistry Print Report · For research reference only
Methyldichlorosilane → Dichloro(3-phenylpropyl)silane
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Methyldichlorosilane | HCID 6376 | — |
| Reactant | Styrene | HCID 7501 | — |
| Reactant | Sodium caprylyl sulfonate | HCID 23669624 | — |
| Catalyst | Platinum | HCID 23939 | — |
| Solvent | Toluene | HCID 1140 | — |
| Product | Dichloro(3-phenylpropyl)silane | HCID 71431464 | 46% |
Reaction Steps
Reaction between styrene and methyldichlorosilane with platinum catalyst in the presence of sodium 1-octanesulfonate. 624 mg Styrene and 732 mg methyldichlorosilane were introduced into a glass tube, and 40 mg of sodium 1-octanesulfonate were added. 0.9 mg Of a toluene solution of a 0-valent platinum complex of divinylsiloxane (0.4 wt % platinum content) was added. The tube was sealed and placed in a 100° C. oil bath where it was heated for 20 hours. After cooling, the tube contents were analyzed by gas chromatography revealing a styrene conversion of 71% and a phenethylmethyldichlorosilane yield of 46%. The ratio between the phenethylmethyldichlorosilane and the (α-methylbenzyl)methyldichlorosilane was 18:1.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US06326506B1 |
| Source dataset | uspto-grants-2001_12 |
| ORD ID | ord-3e02e418d4a648cf93f95ae2a1ec2101 |
| Source note | uspto-grants-2001_12 |