Ethylene Glycol → Dimethyl terephthalate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Ethylene Glycol | HCID 174 | — |
| Reactant | Glycerol | HCID 753 | — |
| Product | Dimethyl terephthalate | HCID 8441 | 380.5% |
Reaction Steps
A polyester produced in known manner from 353 g of dimethyl terephthalate, 153 g of ethylene glycol and 88 g glycerin is heated to 80° C. with the addition of 52 g of cresol. After the further addition of 200 g of trimellitic acid anhydride and 103 g of 4,4'-diaminodiphenylmethane the reaction mixture is further heated, whereby at a temperature of 140° C. the diimidodicarboxylic acid of Example A separates. After further temperature increase esterification occurs at 215° C., until the resin becomes clear. After the addition of 350 g of technical cresol the mixture is cooled to 80° C.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US04267232 |
| Source dataset | uspto-grants-1981_05 |
| ORD ID | ord-96e9b0832b3041e38838d4a55053fe43 |
| Source note | uspto-grants-1981_05 |