Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2286815Generated: October 27, 2026

Acrylamide → Acrylamide

https://huagongshe.com/reaction/2286815

Reaction equation

Participants

RoleNameHCIDCharge
ReactantAcrylamideHCID 6579—
ReactantAcrylic AcidHCID 6581—
ReactantSodium HydroxideHCID 14798—
ReactantAcrylateHCID 25188—
ReactantAmmonium PersulfateHCID 62648—
ReactantSodium Lauryl SulfateHCID 3423265—
SolventAcetoneHCID 180—
SolventMethanolHCID 887—
ProductAcrylamideHCID 6579—
ProductSodium acrylate 2-hydroxypropyl acrylateHCID 86737734—

Reaction Steps

A terpolymer of sodium acrylate-2-hydroxypropyl acrylate and acrylamide was prepared utilizing an emulsion polymerization process. The mole ratios of acrylic acid to acrylamide, mole percent of 2-hydroxypropyl, acrylate and molecular size were varied by controlling the reaction parameters. Six representative samples of the terpolymer were prepared with the compositions of the various terpolymers being estimated based upon their total nitrogen content. In the reaction, ammonium persulfate was utilized as the polymerization initiator or catalyst. Reagent grade acetone and reagent grade anhydrous methanol were utilized to form the solvent. The emulsifier was sodium lauryl sulfate, and 2N aqueous sodium hydroxide was utilized to neutralize the reactants. The dried products were thereafter milled and passed through a number 30 mesh screen. The reaction was conducted over a period of three hours at a reaction temperature of about 60° C.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04268400
Source datasetuspto-grants-1981_05
ORD IDord-d4f703fa60a74fc3bdd4d78a0b7d7d8d
Source noteuspto-grants-1981_05