Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2295525Generated: November 1, 2026

Water → Acrylamide

https://huagongshe.com/reaction/2295525

Reaction equation

Participants

RoleNameHCIDCharge
ReactantWaterHCID 962—
ReactantStyreneHCID 7501—
ReactantAmmonium PersulfateHCID 62648—
Solventtert-ButanolHCID 6386—
ProductAcrylamideHCID 6579—
ProductStyreneHCID 7501—

Reaction Steps

A copolymer of acrylamide (95.0 wt. %) and styrene (5.0 wt. %) is prepared according to a modification of the procedure of Example 1C using 0.5 wt. % n-C12SH, 0.2 wt. % ammonium persulfate and a solvent medium consisting of 75 wt. % deionized water and 25 wt. % t-butanol. The modification is that the styrene monomer is mixed into the chain transfer agent solution and fed into the reaction flask in that solution. Upon completion of the polymerization, the t-butanol is removed via a steam sparge to afford the product at 17.0% solids in water with a Brookfield Viscosity of 28,000 cps.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04425469
Source datasetuspto-grants-1984_01
ORD IDord-d3796363bc264f7eb841f1e9ab0a9228
Source noteuspto-grants-1984_01