Photopolymer plates based on a terpolymer of butadiene, acrylonitrile and acrylic acid were processed as in Example 1 with this solvent. Wash time for this type plate in this wash solution was 16 minutes. Plate exposure times equivalent to those required for perchloroethylene-n-butanol washed plates were necessary to hold 0.004" lines and 3%, 150 line half tones with this wash solvent.
WORKUP
后处理
- washWash time for this type plate in this wash solution