Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Water | HCID 962 | — |
| Reactant | Phosphoric Acid | HCID 1004 | — |
| Reactant | Calcium Hydroxide | HCID 6093208 | — |
| Solvent | Acetic Acid | HCID 176 | — |
| Product | Tricalcium Phosphate | HCID 24456 | — |
Reaction Steps
A new and useful method for producing commercial tri-calcium phosphate, or TCP, utilizes less water and energy than current methods. TCP has the following chemical formula: Ca3(PO4)2. The processes &the present invention produce a TCP product with less energy and less waste than the current methods. According to the method of the present invention in FIG. 1, water 1, hydrated lime 2, related ingredients such as acetic acid 4, and phosphoric acid 3 are admixed in a reaction vessel 7 to form a tri-calcium phosphate slurry 6. The resultant slurry 6 has approximately 72% water and 28% by weight of solid TCP. The slurry 6 then physically contacts air to remove the moisture from the slurry 6. To remove the moisture, the air temperature must reach the evaporation point of the moisture in the slurry 6. The heat of the chemical reaction is controlled to produce TCP having certain characteristics, such as fine particle or powdery form.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US07754174B2 |
|---|
| Source dataset | uspto-grants-2010_07 |
|---|
| ORD ID | ord-2f889752971a493784bf763d95f42844 |
|---|
| Source note | uspto-grants-2010_07 |
|---|