Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | 2-Methyl-2-butanol | HCID 6405 | — |
| Reactant | Trimethylolethane | HCID 6502 | — |
| Reactant | 2-(Dimethylamino)-2-methylpropanol | HCID 23435 | — |
| Reactant | Diacetone Alcohol | HCID 31256 | — |
| Reactant | Acetylacetone | HCID 31261 | — |
| Catalyst | Tin atom | HCID 5352426 | — |
| Solvent | Water | HCID 962 | — |
| Solvent | Methyl Ethyl Ketone | HCID 6569 | — |
| Solvent | N-methyl-2-pyrrolidone | HCID 13387 | — |
| Product | Trimethylolethane | HCID 6502 | — |
| Product | Triethanolamine | HCID 7618 | — |
Reaction Steps
22.4 g DP9C/012, 3.9 g Poly G 83-34, 1.0 g Pluronic L-62, 0.4 g trimethylolethane, 2.0 g Cirrasol G-265, 1.0 g DMAMP DBS, and 0.11 g tin catalyst are added to 2.6 g N-methyl pyrrolidone plus 4.7 g methylethylketone, 2.8 g tertiary amyl alcohol, 0.6 g 2,4-pentanedione and 4.0 g diacetone alcohol and are mixed together. The mixture is heated to 60° C. and then reacted for 6 hours in a nitrogen atmosphere. Following the reaction, the resulting polyurethane prepolymer mixture is cooled and then dispersed in 59.0 g of distilled water, 0.1 g trimethylolethane, and 0.2 g triethanolamine with a high shear disperser, resulting in a stable aqueous polyurethane dispersion having about 24% solids by weight of the dispersion. The resulting polyurethane comprises about 3% polyethylene oxide side chains by weight of the solids of the polyurethane, about 12% polyethylene oxide main chains by weight of the solids of the polyurethane, and about 48% blocked polyisocyanates by weight of the solids of the polyurethane.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08642180B2 |
|---|
| Source dataset | uspto-grants-2014_02 |
|---|
| ORD ID | ord-265729087b3b4af0b137e6e51302343a |
|---|
| Source note | uspto-grants-2014_02 |
|---|