Back
HuagongsheHuagongshe Chemistry Print Report · For research reference only
HRID 2374656Generated: October 30, 2026

6-Aminohexanoic Acid → Nylon 6/66

https://huagongshe.com/reaction/2374656

Reaction equation

Participants

RoleNameHCIDCharge
Reactant6-Aminohexanoic AcidHCID 564—
ReactantCaprolactamHCID 7768—
ReactantHexamethylenediamine adipateHCID 197024—
ProductNylon 6/66HCID 168236—

Reaction Steps

Any method known in the art can be used to produce the polyamides. The polyamides are generally prepared by melt phase polymerization from a diacid-diamine complex which may be prepared either in situ or in a separate step. In either method, the diacid and diamine are used as starting materials. Alternatively, an ester form of the diacid may be used, preferably the dimethyl ester. If the ester is used, the reaction must be carried out at a relatively low temperature, generally 80 to 120° C., until the ester is converted to an amide. The mixture is then heated to the polymerization temperature. In the case of polycaprolactam, either caprolactam or 6-aminocaproic acid can be used as a starting material and the polymerization may be catalyzed by the addition of adipic acid/hexamethylene diamine salt which results in a nylon 6/66 copolymer. When the diacid-diamine complex is used, the mixture is heated to melting and stirred until equilibration.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS07462684B2
Source datasetuspto-grants-2008_12
ORD IDord-8014fb78ce0e474abcaac6c1033176cd
Source noteuspto-grants-2008_12