HCID 21583954, compound → Methyl Salicylate
Reaction equation
C(O)C.O.[C:5]([O:14][CH3:15])(=[O:13])[C:6]1[C:7](=[CH:9][CH:10]=[CH:11][CH:12]=1)[OH:8].[NH2+]1CCN=C1>CCOCC>[C:5]([O:14][CH3:15])(=[O:13])[C:6]1[C:7](=[CH:9][CH:10]=[CH:11][CH:12]=1)[OH:8]Participants
Reactant 2
Product 1
Reagents, catalysts & solvents 1
Conditions
- Temperature
- 70 °C
Procedure
740 Grams of a mixed solvent of ethanol/water/methyl salicylate=60/30/10 was added to 100 g of a polymer solution (polymer concentration: about 42%) substituted with imidazolinium cations obtained as in Example 4, to dissolve the polymer, to obtain a solution having the polymer concentration of 5%. To 100 g of this mixed solution was added 0.5 g of the aforementioned polyglycerolpolyglycidyl ether (described-above) used in Example 4, this was placed into a 100 ml sample bottle, the sample bottle was sealed, the bottle was heated for 1 hour in a constant temperature bath at 70° C. to gelate the material, to obtain the integrated gelated-type patch material (RC1) of the present invention with methyl salicylate-based percutaneous absorption drug absorbed therein.
Workup
- customobtained as in Example 4
- dissolutionto dissolve the polymer
- customto obtain a solution
- customthe sample bottle was sealed
Sources & evidence
- ORD record
- ord-60ee426752024b22b2a553937be5f4dd
- Source dataset
- uspto-grants-2008_12
- Patent number
- US07470738B2
Reaction notes