Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)

HRID 2380373Notes

Reaction equation

HRID 2380373 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9](#[N:12])[CH:10]=[CH2:11]>>[CH2:11]=[CH:10][C:9]#[N:12].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1

Participants

3

Procedure

ABS-2 a graft copolymer obtained by grafting 26.5 parts by weight of styrene and 8.3 parts by weight of acrylonitrile on 65.2 parts by weight of a polybutadiene latex. The content of non-grafted styrene-acrylonitrile copolymer (SAN) obtained in the grafting reaction of the isolated ABS was approximately 6.3% by weight. The weight ratio styrene to acrylonitrile in the SAN was approximately 2.7. The weight-averaged molecular weight of the SAN was approximately 78,000. The particle size of the butadiene rubber is indicated in the appended Figure and in the table hereinafter. The gel content was 95% by weight.

Workup

  1. customABS-2 a graft copolymer obtained

Sources & evidence

ORD record
ord-f82a150899a8461faef4f94f34c8c97a
Source dataset
uspto-grants-1994_11
Patent number
US05367021

Reaction notes