Styrene → Prop-2-enenitrile--ethenylbenzene (1/1)

HRID 2380374Notes

Reaction equation

HRID 2380374 reaction equation
[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1.[C:9](#[N:12])[CH:10]=[CH2:11]>>[CH2:11]=[CH:10][C:9]#[N:12].[CH2:1]=[CH:2][C:3]1[CH:8]=[CH:7][CH:6]=[CH:5][CH:4]=1

Participants

3

Procedure

ABS-3 a graft copolymer obtained by grafting 25.4 parts by weight of styrene and 7.1 parts by weight of acrylonitrile on 67.5 parts by weight of a polybutadiene latex. The content of non-grafted styrene-acrylonitrile copolymer (SAN) obtained in the grafting reaction of the isolated ABS was approximately 8% by weight. The weight ratio styrene to acrylonitrile in the SAN was approximately 2.8. The weight-averaged molecular weight of the SAN was approximately 108,000. The particle size of the butadiene rubber is recorded in the appended Figure and in the table hereinafter. The gel content was 95% by weight.

Workup

  1. customABS-3 a graft copolymer obtained

Sources & evidence

ORD record
ord-dfec926bdf13422585f02ca05c30b0f0
Source dataset
uspto-grants-1994_11
Patent number
US05367021

Reaction notes

Loading…