참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Methacrylic Acid | HCID 4093 | — |
| 반응물 | Styrene | HCID 7501 | — |
| 반응물 | Ammonium Persulfate | HCID 62648 | — |
| 반응물 | Sodium | HCID 5360545 | — |
| 반응물 | Methacrylic acid ethylene oxide | HCID 21880491 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | 2-Methylprop-2-enoic acid;styrene | HCID 165730 | — |
| 생성물 | Sodium | HCID 5360545 | — |
| 생성물 | Methacrylic acid ethylene oxide | HCID 21880491 | — |
반응 단계
A reaction vessel equipped with a stirring rod and a thermometer was charged with 683 parts by mass of water, 11 parts by mass of a sodium salt of sulfuric acid ester of methacrylic acid-ethylene oxide adduct (ELEMINOL RS-30, manufactured by Sanyo Chemical Industries, Ltd.), 138 parts by mass of styrene, 138 parts by mass of methacrylic acid, and 1 part by mass of ammonium persulfate, and the resulting mixture was stirred for 15 minutes at 400 rpm to thereby prepare a white emulsion. The obtained emulsion was heated until the internal system temperature reached 75° C., and then was allowed to react for 5 hours. To the resultant, 30 parts by mass of a 1% by mass ammonium persulfate aqueous solution was further added, and the resulting mixture was aged for 5 hours at 75° C., to thereby obtain an aqueous dispersion liquid of a vinyl resin (a copolymer of styrene/methacrylic acid/a sodium salt of sulfuric acid ester of methacrylic acid-ethylene oxide adduct), i.e. Particle Dispersion Liquid 1.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US08795938B2 |
|---|
| 출처 데이터셋 | uspto-grants-2014_08 |
|---|
| ORD ID | ord-777b6e478d7449c7a6262b3c65764c35 |
|---|
| 출처 메모 | uspto-grants-2014_08 |
|---|