Participants
| Role | Name | HCID | Charge |
|---|
| Reactant | Carbon Dioxide | HCID 280 | — |
| Reactant | Calciumoxide | HCID 6850728 | — |
| Reactant | Magnesium monoxide | HCID 6850729 | — |
| Solvent | Water | HCID 962 | — |
| Product | Calcium bicarbonate | HCID 10176262 | — |
Reaction Steps
The said calcination process is to calcine the minerals at 700˜1000° C. for 1˜5 hours. The said hydration process is to add water into the magnesium oxide and/or calcium oxide obtained from the calcination to carry out hydration, the hydration temperature is 50˜95° C., the hydration time is 0.5˜5 hours, and the weight ratio of water to magnesium oxide and/or calcium oxide is 1˜5:1, and subsequently, water is further added to prepare slurry at the weight ratio of water to magnesium oxide and/or calcium oxide of 10˜200:1. The said carbonation process is performed after the hydration, carbon dioxide is pumped into the slurry to carry out carbonation, the temperature is controlled at 0˜50° C., the reaction time is 0.1˜5 hours. And after filtration, pure magnesium bicarbonate and/or calcium bicarbonate solution is obtained.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patent number | US08808660B2 |
|---|
| Source dataset | uspto-grants-2014_08 |
|---|
| ORD ID | ord-693dfcead77e473793864cbb330c2349 |
|---|