HuagongsheHuagongshe Chemistry Print Report · For research reference only
Carbon Dioxide → Magnesium bicarbonate
Participants
| Role | Name | HCID | Charge |
|---|---|---|---|
| Reactant | Carbon Dioxide | HCID 280 | — |
| Reactant | Magnesium monoxide | HCID 6850729 | — |
| Solvent | Water | HCID 962 | — |
| Product | Magnesium bicarbonate | HCID 102204 | — |
Reaction Steps
Sodium hydroxide (30%) is added into a magnesium nitrate solution (5.0 mol/L, MgO content: 200 g/L) at a molar ratio of sodium to magnesium of 2. Controlling the reaction for 25 minutes at 20° C., a magnesium hydroxide slurry can be obtained. After filtration, a filter cake of magnesium hydroxide is obtained. Then water is added into the filter cake to prepare slurry at a weight ratio of water to magnesium oxide of 30:1. After that, carbon dioxide (90 vt %) is introduced into the slurry to carry out carbonation at 25° C. Subsequently, a magnesium bicarbonate solution (MgO: 30 g/L, Fe: 0.3 ppm, Al: 0.4 ppm) is obtained after clarification and filtration.
Provenance & Evidence
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patent number | US08808660B2 |
| Source dataset | uspto-grants-2014_08 |
| ORD ID | ord-0f138255849d4fc1b2da3b2e8292abac |
| Source note | uspto-grants-2014_08 |