Ethylene carbonate → Ethylene carbonate

https://huagongshe.com/reaction/247714

Reaction equation

Participants

RoleNameHCIDCharge
ReactantEthylene carbonateHCID 7303—
CatalystSodium StannateHCID 21977542—
ProductCarbon DioxideHCID 28018.7%
ProductEthylene carbonateHCID 730397.3%

Reaction Conditions

Temperature175 °C

Reaction Steps

A 10:1 mole ratio of ethylene carbonate to polyester poly (Formrex® 11-225, a hydroxyl functional diethylene glycol adipate, MW=500, manufactured by Witco) is heated with stirring under a nitrogen atmosphere for 3.5 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 97.3 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 18.7 percent carbon dioxide. The catalyst was removed as in Example 1.

Provenance & Evidence

DOI10.6084/m9.figshare.5104873.v1
Patent numberUS04709069
Source datasetuspto-grants-1987_11
ORD IDord-ee50f29d4fd6404fa60c2a7c438397ec
Source noteuspto-grants-1987_11